Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3X2G10 - PA66-GF50 FR(52) - BASF

Material Data Center offers the following functions for Ultramid® A3X2G10:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Glass fibre fibre reinforced injection moulding grade with improved flame retardance. Flame retardant based on red phosphorus; giving outstanding electrical properties and very high stiffness and strength.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 25 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carico 5 / * kg -
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 16000 / 12000 MPa ISO 527
Carico unitario a rottura 180 / 130 MPa ISO 527
Deformazione a rottura 2 / 3 % ISO 527
Modulo di scorrimento a trazione, 1000h * / 5400 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C 55 / 55 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 50 / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 13 / 16 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 11 / - kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 260 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 250 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 250 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 17 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 66 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco a spessore h V-2 / * class IEC 60695-11-10
Spessore provato 0.4 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco 5V a spess. h 5VA / * class IEC 60695-11-20
Spessore provato 1.6 / * mm -
Yellow Card disponibile sì / * - -
Indice di ossigeno 27 / * % ISO 4589-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 3.6 / 5 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 200 / - E-4 IEC 62631-2-1
Resistività volumica 1E13 / 1E10 Ohm*m IEC 62631-3-1
Resistività superficiale * / 1E13 Ohm IEC 62631-3-2
Rigidità dielettrica 33 / 30 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali - / 600 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 4 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.9 / * % Sim. alla ISO 62
Massa volumica 1600 / - kg/m³ ISO 1183
Proprietà Specifiche Materialesecco/condUnitáNorma del test
ISO Data
Numero di viscosità 140 / * cm³/g ISO 307, 1157, 1628
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 - 100 °C -
Pre-essiccamento - Tempo 4 h -
Umidità del Processo ≤0.15 % -
Temperatura di fusione 290 - 300 °C -
Temperatura dello stampo 80 - 90 °C -
Funzioni
Viscosità-Velocità di taglio , Ultramid® A3X2G10, PA66-GF50 FR(52), BASF
Sforzo di taglio-Velocità di taglio , Ultramid® A3X2G10, PA66-GF50 FR(52), BASF
Modulo dinamico a taglio-temperatura , Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Sforzi-deformazione , Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Sforzi-deformazione , Ultramid® A3X2G10 (cond.), PA66-GF50 FR(52), BASF
Modulo secante-deformazione , Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Modulo secante-deformazione , Ultramid® A3X2G10 (cond.), PA66-GF50 FR(52), BASF
Sforzi-deformazioni (isocrona) 23°C, Ultramid® A3X2G10 (cond.), PA66-GF50 FR(52), BASF
Modulo di scorrimento-tempo 23°C, Ultramid® A3X2G10 (cond.), PA66-GF50 FR(52), BASF
Curva di scorrimento 23°C, Ultramid® A3X2G10 (cond.), PA66-GF50 FR(52), BASF
Sforzi-deformazioni (isocrona) 60°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Modulo di scorrimento-tempo 60°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Curva di scorrimento 60°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Sforzi-deformazioni (isocrona) 90°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Modulo di scorrimento-tempo 90°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Curva di scorrimento 90°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Sforzi-deformazioni (isocrona) 120°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Modulo di scorrimento-tempo 120°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Curva di scorrimento 120°C, Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Volume specifico-temperatura (pvT) , Ultramid® A3X2G10, PA66-GF50 FR(52), BASF
Modulo a taglio-temperatura , Ultramid® A3X2G10 (Secco), PA66-GF50 FR(52), BASF
Modulo a taglio-temperatura , Ultramid® A3X2G10 (cond.), PA66-GF50 FR(52), BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Stabilizzato o stabile al calore
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 100 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 290 - 300 °C
injection molding, Melt temperature, recommended: 295 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 85 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.